Through the previous several issues, we learned the characteristics of high-frequency welding process related factors, this issue we summarize the welding process. In high frequency welding, the influence of welding speed on welding process should be reflected in extrusion roll forming elements, material characteristics elements, welding power elements, welding frequency elements and welding speed elements, We can conclude that the main purpose of welding process is to control two contents: the size of heat affected zone (the volume of heated material in extrusion zone) and the heating time of heat affected zone.
1. Size of heat affected zone
In the process of high frequency welding, the size of heat affected zone directly affects the quality of welding products, which is very important; If the heat affected zone is too small, the weld fusion is insufficient and the welding is unqualified. Only suitable size of heat affected zone can get suitable weld and qualified product.
2. Heating time
In high frequency welding, the length of heating time is a direct factor affecting the microstructure characteristics of heat affected zone (HAZ), which is also very important. The length of heating time has a significant impact on the grain structure of the material in the melting zone. The appropriate grain structure and thermal streamline are the key to ensure that the weld microstructure is comparable to the base metal, High frequency welding must require that the microstructure of the weld is better than that of the base metal, which requires that the microstructure and properties of the weld must be guaranteed. Therefore, high frequency welding usually requires a certain welding speed, which should not be too low. If the heating time is too long, it will not only affect the size of the heat affected zone, but also affect the grain size, resulting in grain growth, affecting the performance of the weld, which may have obvious adverse effects in some weld performance experiments. Of course, if the heating time is too short, it will cause cold welding if it is not heated thoroughly, which makes it impossible to complete the welding effect. Therefore, the heating time is also the key.