In the products with high-frequency welding of pipes, when debugging the products with small pipe diameter, especially the products with pipe diameter less than 1 / 2 ", and the wall thickness is very thin, and the wall thickness is 1mm or less, when the steel strip enters the extrusion rod after passing through the high-frequency induction coil, sometimes the steel strip on both sides of the triangle area cannot be extruded, that is, the edges on both sides are misaligned, which is called edge rolling.
Reasons for this phenomenon:
1. The wall thickness of pipe specification is too thin;
2. The overall torsional strength of raw materials with small pipe diameter is not high;
3. High speed welding process;
The above reasons are the objective factors of edge frustration in the process of high frequency welding.
How to avoid this phenomenon? Technical workers suggest the following measures:
1. Try to shorten the space distance between the extrusion rod and the last forming rod (guide rod) immediately following it;
2. Adjust the appropriate extrusion force;
3. Minimize the width of heat affected zone of high-frequency welding (methods have been communicated with you in the previous article);
4. For the triangular zone of the high-frequency welding zone of the extrusion rod, it is very important for the steel strip to maintain a certain stable tension in the three-dimensional space